Export compliance
Heat-treated pallets, IPPC-stamped, with treatment records
If your freight leaves the United States, the wood under it must be heat-treated to the ISPM-15 standard and carry a registered IPPC mark. Partner suppliers in our network supply HT-stamped stock from registered facilities, with the paperwork — so a customs hold never starts with your pallet.
Short answer
ISPM-15 requires a 56 °C core temperature held for 30 continuous minutes, verified by probe, followed by an IPPC stamp showing country, facility code and treatment type (HT).
Domestic-only freight does not need it. Heat treatment adds to the unit price; partner suppliers quote it alongside the pallets.
How the treatment actually runs
Probe in the thickest board, not a guess at the air temperature
The standard is about wood core temperature, which is why cheap 'HT' pallets fail inspection. Air temperature in a chamber tells you nothing about the middle of a 3.5-inch stringer.
- 01
Pre-sort and moisture check
Units are graded first. There is no point treating a pallet that will be rejected on condition anyway.
- 02
Load the chamber
Stacks are spaced for airflow. Tight-packed loads leave cold spots in the middle of the stack.
- 03
Probe placement
Calibrated probes go into the thickest stringer of the coldest-expected position, not the convenient one.
- 04
Ramp and hold
Chamber ramps until every probe reads 56 °C core, then the 30-minute clock starts. Any dip restarts it.
- 05
Chart logging
Time and temperature are logged for the whole run. That chart is your evidence.
- 06
Cool and stamp
Units are stamped with the treating facility's registered code, country code US and the HT mark on two opposing stringers.
- 07
Segregate
Treated stock is stored separately from untreated. Cross-contamination of stacks is how compliance quietly fails.
- 08
Document
Treatment certificate, run chart and unit count supplied with the delivery note.
Key takeaways
- ISPM-15 applies to the packaging, not the goods — a compliant product on a non-compliant pallet is still rejected.
- Heat treatment is not kiln drying. KD is a moisture spec; HT is a phytosanitary spec. A pallet can be one without the other.
- Methyl bromide (MB) fumigation is being phased out globally. Ask for HT stock instead.
- Debarked wood is also required — bark on a stringer fails inspection even after valid treatment.
Reading the stamp
What each element of an IPPC mark means
| Element | Example | Meaning |
|---|---|---|
| IPPC symbol | Wheat sheaf logo | Mandatory. Confirms the mark is a phytosanitary one. |
| Country code | US | ISO two-letter code of the treating country. |
| Facility code | CO-#### | State abbreviation plus the registered facility number. |
| Treatment code | HT | HT = heat treatment. DH = dielectric heating. MB = methyl bromide (avoid). |
| Placement | Two opposing sides | Must be visible, legible and permanent — stencilled or branded, never a sticker. |
If a pallet shows an MB mark, many destinations will now refuse it outright. If it shows no mark at all, assume it is domestic-only stock.
Pricing and lead time
What drives an export-ready quote
Heat-treated stock is priced by quote from partner suppliers. The base pallet, the kiln run and the paperwork all feed into it, and the supplier confirms the lead time.
| Product | What sets the price | What sets the lead time |
|---|---|---|
| 48×40 reclaimed Grade A + HT | Grade, count, kiln run | Stock on hand and kiln schedule |
| 48×40 new stringer + HT | Lumber, build, kiln run | Saw line and kiln schedule |
| 48×40 new block + HT | Lumber, build, kiln run | Saw line and kiln schedule |
| Custom build + HT | Design, lumber, kiln run | Design sign-off, build and kiln |
| Export crate + HT | Design and materials | Design, build and treatment |
| Treat customer-owned stock | Run size and handling | Facility schedule |
Treating your own pallets is a real option — some registered partner facilities will run, stamp and document customer-owned stock, usually with a minimum run size.

Where the stamp gets read
A customs officer has one question
Is the wood debarked, treated and marked? Everything upstream — probe placement, the 30-minute hold, the chart record, the segregated bay — exists so that the answer is yes at a terminal on the other side of the world, long after anybody at the treating facility could do anything about it.
Compliance questions
The ones that avoid a customs hold
Does Canada or Mexico require ISPM-15 from the US?
Wood packaging moving between the US and Canada has long had an exemption, but the rules for Mexico differ, and individual commodities, customers and carriers can still demand compliance. Check current regulations with your forwarder or the destination's plant health agency. If the freight is valuable or time-critical, treat it — treatment costs far less than a day held at a border.
Can I just re-use a pallet that already has an HT stamp?
Yes, provided the pallet has not been repaired with untreated lumber since. Any repair with untreated wood voids the mark — the unit must be re-treated and re-stamped. A well-run repair line keeps treated and untreated board stock physically separate for exactly this reason.
How long is a heat treatment valid for?
Indefinitely, as long as the wood is not re-infested or repaired with untreated material. There is no expiry date in the standard. Practically, a stamp that is no longer legible is a stamp that does not exist.
What about plywood, OSB and engineered crating?
Manufactured wood products processed with heat and glue — plywood, OSB, LVL, hardboard — are exempt from ISPM-15. Solid wood frames and skids on the same crate are not. Mixed crates are where most compliance failures happen; see custom crating.
By destination
Where ISPM-15 bites, and where it does not
The standard is adopted very widely, but the practical questions are narrower: does your destination accept methyl bromide, how closely does it inspect, and what happens if wood fails. Requirements change, so check current regulations for each lane.
| Question | Why it matters |
|---|---|
| Is ISPM-15 treatment required? | Almost every destination outside North America requires it |
| Is methyl bromide accepted? | A growing number of destinations refuse MB-marked wood |
| How closely does it inspect? | Some ports inspect wood packaging far more often than others |
| What happens if wood fails? | Outcomes range from treatment at port to destruction or re-export |
| Does the freight continue onward? | An onward leg can bring in a stricter destination's rules |
The treatment record
What to ask for with the delivery
A compliant pallet and a defensible pallet are different things. The mark satisfies an inspector at a glance; the paperwork settles a dispute.
Documentation to ask the supplier for
Reputable HT suppliers provide this with the delivery note and keep it on file.
- Treatment certificate naming the registered facility code
- Time-and-temperature chart for the whole kiln run
- Probe placement record for that run
- Unit count treated and the order it belongs to
- Confirmation of debarking at intake
- Stamp placement record — two opposing stringers
- Statement that no methyl bromide was used
Treatment parameters
- Standard
- ISPM-15, treatment code HT
- Core temperature
- 56 °C minimum
- Hold time
- 30 continuous minutes
- Verification
- Calibrated probes, thickest member
- Chart logging
- Full run, time and temperature
- Debarking
- Required and verified at intake
- Mark placement
- Two opposing faces, permanent
- Minimum run
- varies by facility
- Methyl bromide
- Avoid — ask for HT
Exemptions
What does not need treating — and the trap inside the list
Manufactured wood products are exempt because the manufacturing process already destroys pests. The exempt list is generous, and mixed-material crates are where compliance most often quietly fails.
| Material | In scope? | Note |
|---|---|---|
| Solid wood pallets and skids | Yes | Treatment and IPPC mark required |
| Solid wood crate frames and cleats | Yes | Even under exempt sheathing |
| Dunnage, blocking and bracing timber | Yes | Frequently overlooked |
| Plywood | No | Manufactured with heat, glue and pressure |
| OSB and particleboard | No | Exempt |
| LVL and engineered beams | No | Exempt |
| Hardboard and veneer | No | Exempt |
| Wood thinner than 6 mm | No | Exempt by thickness |
| Sawdust, shavings, wood wool | No | Exempt |
| Wine and spirit barrels, heated | No | Exempt |
| Gift boxes, manufactured pest-free | No | Exempt |
| Plastic and metal pallets | No | Outside the standard entirely |
| Presswood / moulded pallets | No | Manufactured with heat and pressure |
| Permanent vehicle and container timber | No | Exempt |
Why wood gets rejected
Six common failures
- 01
Bark left on a stringer or block
ISPM-15 requires debarked wood. Bark harbours pests that treatment may not reach, so residual bark fails inspection even after a perfectly valid kiln run.
Instead: Good facilities verify debarking at intake, before anything enters the chamber. If you are treating your own stock, make it the first check.
- 02
An illegible or single-sided mark
Stencils fade, labels get stuck over them, and a mark applied to one face disappears the moment the pallet is loaded and that face is against a wall.
Instead: Two opposing faces, permanent application — stencilled or branded, never a sticker. Ask for both to be placed and recorded.
- 03
Repaired with untreated lumber after treatment
It voids the mark. The pallet looks perfect, the stamp is legible, and the unit is non-compliant. Inspectors look for mismatched board colour.
Instead: Keep treated and untreated board stock physically separated by location, not by label. Re-treat and re-stamp anything repaired.
- 04
An MB mark at a destination that now refuses it
Methyl bromide was a valid treatment when applied and is being phased out under the Montreal Protocol. The list of destinations refusing it grows, and the mark is permanent.
Instead: Specify HT explicitly rather than 'ISPM-15 compliant'. A registered HT facility can heat treat and re-stamp MB stock, which supersedes the original mark.
- 05
A solid frame under exempt sheathing, unmarked
The plywood is exempt, the frame is not, and the assembled crate carried no mark because somebody checked only the outside material.
Instead: Treat and mark any crate with solid wood structure, regardless of what it is clad in.
- 06
A live pest found despite a valid mark
A compliant mark does not override an insect in the wood. This is the outcome that can condemn an entire consignment rather than just its packaging.
Instead: Store treated stock under cover and away from untreated timber. Re-infestation after treatment is rare but it is the one failure with no appeal.
Shipping abroad next month?